Posted 19 November 2016 - 04:58 AM

I have a kettle I don't really use but I was thinking I could sell it on the cheap to someone I know that wants to start brewing.

Only issue is that there is a little bit of galvanic corrosion (or it at least looks like it) around the handle rivets. The kettle itself is SS. I'm not sure what the rivet is. The rivet has some white corrosion that builds up on it.

Any way to stop this? Is this corrosion going to add anything concerning to the beer if it falls in?

#2 3rd party JKor

3rd party JKor

    Puller of Meats

  • Patron
  • PipPipPipPipPipPip
  • 64137 posts
  • LocationNW of Boston

Posted 20 November 2016 - 09:20 AM

It will definitely kill you.



#3 positiveContact

positiveContact

    Anti-Brag Queen

  • Patron
  • PipPipPipPipPipPip
  • 68886 posts
  • LocationLimbo

Posted 20 November 2016 - 01:09 PM

doh!



#4 positiveContact

positiveContact

    Anti-Brag Queen

  • Patron
  • PipPipPipPipPipPip
  • 68886 posts
  • LocationLimbo

Posted 21 November 2016 - 09:03 AM

so any ideas here?  is there no way to stop this corrosion from continuing?



#5 3rd party JKor

3rd party JKor

    Puller of Meats

  • Patron
  • PipPipPipPipPipPip
  • 64137 posts
  • LocationNW of Boston

Posted 21 November 2016 - 11:56 AM

Install an anode in the kettle?

Otherwise probably not. I don't think its a big deal, just scrub it after each batch.

#6 dmtaylor

dmtaylor

    Advanced Member

  • Members
  • PipPipPip
  • 325 posts
  • LocationTwo Rivers, WI

Posted 22 November 2016 - 09:30 AM

You could coat the rivets with a couple coats of epoxy.  If done right, it would stop the corrosion.  But it would probably make the kettle look even worse.  So, I wouldn't bother.



#7 SchwanzBrewer

SchwanzBrewer

    Grand Duke of Inappropriate Announcements

  • Patron
  • PipPipPipPipPip
  • 34299 posts
  • LocationKnee deep in business plans

Posted 22 November 2016 - 04:42 PM

I wouldn't worry about it. All my cheaper turkey fryer SS pots have that going on. I often soak them in starsan though when I brew so I guess they possibly get passivated a little. Who knows though, I don't let it bother me.